Polymer Property : Compressive Yield Strength = 261000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 1800 MPa
261000 psi
0.2%, hardened to 55 HRC
Bohler-Uddeholm AISI A2 Cold Work Tool Steel
Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c..
Compressive Yield Strength 1800 MPa
261000 psi
0.2%, Aged to ~ 50 HRC
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel
A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli..
Compressive Yield Strength 1800 MPa
261000 psi
0.2%, hardened to 55 HRC
Bohler-Uddeholm O1 Cold Work Tool Steel
Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha..