Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 172 MPa | 25000 psi | Unit Load Limit |
Polygon Polylube™ Fiber Series Epoxy Composite Bearings Low friction coupled with high load carrying capacity are natural benefits. Teflon® superfilaments, which exhibit tensile strength twenty times greater than PTFE resins are integrated into the bea.. |
|||
Compressive Yield Strength | 172 - 379 MPa | 25000 - 55000 psi | Average value: 234 MPa Grade Count:13 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Compressive Yield Strength | 172 - 231 MPa | 25000 - 33500 psi | Average value: 192 MPa Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |