Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 162 MPa | 23500 psi | 10% Offset; ASTM D695 |
Cast Nylons Nycast® 6MPB Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Compressive Yield Strength | 162 MPa | 23500 psi | 10% Offset; ASTM D695 |
Cast Nylons Nycast® 6MPY Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Compressive Yield Strength | 162 - 195 MPa | 23500 - 28300 psi | Average value: 177 MPa Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |