Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 160 - 274 MPa | 23200 - 39700 psi | Average value: 208 MPa Grade Count:5 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Compressive Yield Strength | 160 MPa @Strain 10.0 %, Temperature 23.0 °C |
23200 psi @Strain 10.0 %, Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4041 Polyimide, Glossy Black, Molybdenum Sulfide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Compressive Yield Strength | 160 MPa | 23200 psi | ASTM D695 |
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |