Polymer Property : Compressive Yield Strength = 23.2 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.160 MPa
23.2 psi
at 30% deflection; ASTM D3574C
Mearthane Durethaneâ„¢ M DM-720A Foam Polyurethane
MDI backbone: ether.Shore 00 Hardness: 65Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
Compressive Yield Strength 0.160 MPa
23.2 psi
at 5% compression ,after 24 hrs at 1010°C, parallel to thickness
Zircar Refractory Composites RSBD-LD ALUMINA-SILICA INSULATION
ZRCI Alumina-Silica Insulation Type RSBD-LD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a..