Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 150 MPa | 21800 psi | ASTM D695 |
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type.. |
|||
Compressive Yield Strength | 150 MPa | 21800 psi | ASTM D695 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Compressive Yield Strength | 150 MPa | 21800 psi | 0.2% proof |
AMT AM-Lite® Die Casting Magnesium Alloy AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has.. |