Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 14.0 MPa | 2030 psi | at 5% nominal strain; ISO 604 |
Quadrant EPP Cestilene™ HD 1000 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Compressive Yield Strength | 14.0 - 110 MPa | 2030 - 16000 psi | Average value: 60.5 MPa Grade Count:20 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Compressive Yield Strength | 14.0 - 110 MPa | 2030 - 16000 psi | Average value: 61.9 MPa Grade Count:7 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Compressive Yield Strength | 14.0 MPa | 2030 psi | ASTM D395 |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 35 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Compressive Yield Strength | 14.0 MPa @Strain 1.00 % |
2030 psi @Strain 1.00 % |
ISO 604 |
Manifattura Cattaneo PP-s Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |