Mechanical Properties Metric English Comments
Compressive Yield Strength 13.8 MPa
2000 psi
Mixed 1:2; TM R050-38
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Compressive Yield Strength 13.8 MPa
2000 psi
TM R050-38
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive
Resinlab™ EP1290 Clear is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to ..
Compressive Yield Strength 13.8 - 279 MPa
2000 - 40500 psi
Average value: 109 MPa Grade Count:32
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..
Compressive Yield Strength >= 13.8 MPa
>= 2000 psi
Stabilized, min
Hexcel® HexWeb® CR III 1/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength 13.8 MPa
2000 psi
Bare, typ
Hexcel® HexWeb® HRH-10 - 1/8- 9.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength 13.8 MPa
2000 psi
TM R050-38
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive
Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m..
Compressive Yield Strength 13.8 MPa
2000 psi
TM R050-38
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit..