Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1172 MPa | 170000 psi | transverse |
ATI Allegheny Ludlum Stainless Steel Type 301, 3/4 Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |