Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 115 MPa | 16700 psi | |
Epoxy Novolac 27%, Carbon fabric 73% Epoxy Novolac - Dow Chemical "DEN 438". Carbon fabric - "VCA" |
|||
Compressive Yield Strength | 115 MPa | 16700 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre.. |
|||
Compressive Yield Strength | 115 MPa | 16700 psi | Typical averaged test results for Abatron Adhesive/Casting Resins. |
Abatron AboWeld 48-14/AboCure 48-14 Adhesive/Casting Resin Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a.. |
|||
Compressive Yield Strength | 115 MPa | 16700 psi | Typical averaged test results for Abatron Adhesive/Casting Resins. |
Abatron AboWeld 48-8/AboCure 48-8 Adhesive/Casting Resin Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a.. |
|||
Compressive Yield Strength | 115 MPa | 16700 psi | Typical averaged test results for Abatron Adhesive/Casting Resins. |
Abatron AboCast 37-10/AboCure 37-10 Adhesive/Casting Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a.. |
|||
Compressive Yield Strength | 115 MPa | 16700 psi | Typical averaged test results for Abatron Adhesive/Casting Resins. |
Abatron AboCast 45-10/AboCure 45-10 Adhesive/Casting Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a.. |
|||
Compressive Yield Strength | 115 MPa | 16700 psi | Typical averaged test results for Abatron Adhesive/Casting Resins. |
Abatron AboCast 53-15/AboCure 53-15 Adhesive/Casting Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend a.. |