Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 113 MPa | 16400 psi | ASTM D695 |
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren.. |