Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 108 MPa | 15600 psi | ASTM D695 |
Diapolyacrylate Acrypet® VH-001 Heat Stabilized PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |