Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 10.3 MPa @Strain 10.0 % |
1500 psi @Strain 10.0 % |
|
Saint-Gobain Rulon® E Grade Bearing/Seal PTFE
(discontinued **) Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and .. |
|||
Compressive Yield Strength | 10.3 MPa | 1500 psi | Bare, typ |
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Yield Strength | 10.3 MPa | 1500 psi | TM R050-38 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |
|||
Compressive Yield Strength | 10.3 MPa | 1500 psi | Bare, typ |
Hexcel® HexWeb® CR III 1/8-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | 10.3 MPa | 1500 psi | TM R050-38 |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |
|||
Compressive Yield Strength | 10.3 MPa | 1500 psi | Bare, typ |
Hexcel® HexWeb® CR III 1/16-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |