Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 98.94 MPa | 14350 psi | ASTM D695 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Compressive Yield Strength | 98.94 MPa | 14350 psi | ASTM D695 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Compressive Yield Strength | 98.94 MPa | 14350 psi | ASTM D695 |
Westlake Plastics Radel® R Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr.. |