Mechanical Properties Metric English Comments
Compressive Yield Strength >= 0.900 MPa
>= 131 psi
ASTM C365
Parabeam Industrie Paraglass 15 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Compressive Yield Strength 0.900 MPa
131 psi
Typical; ASTM C365
Parabeam Industrie Paraglass 18 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Compressive Yield Strength 0.900 MPa
131 psi
Ultracor® UKF-68-3/8-2.0 Honeycomb Core Material
Construction: ±45° K49 120. Fiber: Kevlar® K49. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be..
Compressive Yield Strength 0.900 MPa
131 psi
Stabilised
Hexcel® HexWeb® CRF-3/4-ACG-.003-1.8 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..