Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0896 MPa | 13.0 psi | At 10% compression |
Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Compressive Yield Strength | 0.0896 MPa | 13.0 psi | At 10% compression |
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Compressive Yield Strength | 0.0896 MPa | 13.0 psi | At 10% compression |
Zircar Zirconia ZYF-A2.13 Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |
|||
Compressive Yield Strength | 0.0896 MPa | 13.0 psi | At 10% compression |
Zircar Zirconia ZYF-S.75G Zirconia Felt Insulation Zirconia Felt is a true ceramic textile formed by the unique ZIRCAR process for replicating organic structures in inorganic materials. The zirconia felt structure is a ‘needled felt’ which retains.. |