Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 7.00 - 9.00 MPa

@Strain 1.00 %
1020 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G416 Polytetrafluoroethylene 40% Bronze, 2% Carbon
PTFE G Special Compound with bronze Properties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard ..
Compressive Yield Strength 8.50 - 9.00 MPa

@Strain 1.00 %
1230 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide
PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon®
Compressive Yield Strength 7.00 - 9.00 MPa

@Strain 1.00 %
1020 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Compressive Yield Strength 8.00 - 9.00 MPa

@Strain 1.00 %
1160 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..
Compressive Yield Strength 7.00 - 9.00 MPa

@Strain 1.00 %
1020 - 1310 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..