Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 76.4919 - 76.5318 MPa @Temperature 149 - 150 °C |
11094.2 - 11100.0 psi @Temperature 300 - 302 °F |
Average value: 76.5 MPa Grade Count:2 |
Overview of materials for Thermoplastic Polyimide, Unfilled |