Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 35.0 - 221 MPa | 5080 - 32000 psi | Average value: 112 MPa Grade Count:10 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Compressive Yield Strength | 124 - 221 MPa | 18000 - 32000 psi | Average value: 182 MPa Grade Count:8 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Compressive Yield Strength | 145 - 221 MPa | 21000 - 32100 psi | Average value: 195 MPa Grade Count:12 |
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Heat Resistant Grade, Filled". Each property range of values reported is minimum and .. |