Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 51.7 - 131 MPa | 7500 - 19000 psi | Average value: 81.6 MPa Grade Count:8 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |