Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0276 - 0.110 MPa @Strain 25.0 % |
4.00 - 16.0 psi @Strain 25.0 % |
0.2"/min. strain rate |
Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade Thickness: 0.062"- 0.188"Color: BlackInformation provided by Rogers Corporation. |