Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 68.9 MPa | 10000 psi | TM R050-38 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Compressive Yield Strength | 68.9 MPa | 10000 psi | TM R050-38 |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Compressive Yield Strength | 68.9 MPa | 10000 psi | TM R050-38 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Compressive Yield Strength | 68.9 MPa | 10000 psi | TM R050-38 |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Compressive Yield Strength | 68.9 - 165 MPa | 10000 - 23900 psi | Average value: 114 MPa Grade Count:20 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Compressive Yield Strength | 68.9 - 179 MPa | 10000 - 26000 psi | Average value: 140 MPa Grade Count:12 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Compressive Yield Strength | 68.9 MPa | 10000 psi | Average value: 68.9 MPa Grade Count:3 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Compressive Yield Strength | 68.9 MPa | 9990 psi | at 5% compression |
Zircar Refractory Composites RS-DR Refractory Sheet TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier f.. |
|||
Compressive Yield Strength | 68.9 MPa | 10000 psi | TM R050-38 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Compressive Yield Strength | 68.9 MPa | 10000 psi | TM R050-38 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |