Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 5.86 MPa | 850 psi | Stabilized, typ |
Hexcel® HexWeb® HRH-10/F50 - 5.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglass cloth reinforc.. |
|||
Compressive Yield Strength | >= 5.86 MPa | >= 850 psi | Bare, min |
Hexcel® HexWeb® HRP/OX - 1/4 - 7.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Compressive Yield Strength | >= 5.86 MPa | >= 850 psi | Bare, min |
Hexcel® HexWeb® HRH-10 - 1/8- 6.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Compressive Yield Strength | 5.86 MPa | 850 psi | |
Aptek DI-STRATE 1500-1 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Iridium Satellite AntennasInformation provi.. |