Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 5.17 MPa | 750 psi | TM R050-38 |
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Compressive Yield Strength | >= 5.17 MPa | >= 750 psi | Stabilized, min |
Hexcel® HexWeb® CR III 3/8-5052-.005 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | >= 5.17 MPa | >= 750 psi | Stabilized, min |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.005 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Yield Strength | >= 5.17 MPa | >= 750 psi | Stabilized, min |
Hexcel® HexWeb® HRP - 3/16 - 5.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Compressive Yield Strength | 5.17 MPa | 750 psi | TM R050-38 |
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Compressive Yield Strength | 5.17 MPa | 750 psi | TM R050-38 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |
|||
Compressive Yield Strength | 5.17 MPa | 750 psi | Max load under tribological use |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |