Mechanical Properties Metric English Comments
Compressive Yield Strength 5.00 MPa
725 psi
at 1% nominal strain; ISO 604
Quadrant EPP Cestlite™ ASTL Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Compressive Yield Strength 5.00 - 15.2 MPa
725 - 2200 psi
Average value: 7.11 MPa Grade Count:6
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Compressive Yield Strength 5.00 - 15.2 MPa
725 - 2200 psi
Average value: 6.57 MPa Grade Count:9
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
Compressive Yield Strength 5.00 - 6.00 MPa

@Strain 1.00 %
725 - 870 psi

@Strain 1.00 %
ASTM D695
Guarniflon PTFE G800 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Compressive Yield Strength >= 5.00 MPa
>= 725 psi
Bare, min, preliminary value obtained from limited testing
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..