Mechanical Properties Metric English Comments
Compressive Yield Strength 47.0 MPa

@Strain 25.0 %
6820 psi

@Strain 25.0 %
Z direction; 0.05/min strain rate; ASTM D695
Rogers Corporation RT/duroid® 6010.2LM Ceramic-PTFE Composite Microwave Laminate
Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowLow Z-axis expansion. Provides reliable plated through holes in multi-layer boardsTight ..