Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 369 MPa | 53500 psi | Compression After Impact @ 6.6 J/mm, Results normalized to 60% fibre volume for Carbon, 50% fibre volume for Kevlar; pr EN 6038 |
Hexcel® HexPly® 920CX-EP2015-47.5% 125°C Curing Epoxy Matrix Intermediate modulus, 6K carbon, 2x2 twill, 193 g/m2Information provided by HexCel |