Polymer Property : Compressive Yield Strength = 33.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 33.0 - 145 MPa
4790 - 21000 psi
Average value: 73.9 MPa Grade Count:12
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Compressive Yield Strength 33.0 - 148 MPa
4790 - 21500 psi
Average value: 87.0 MPa Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..