Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 207.9 MPa | 30150 psi | ASTM D695 |
Plenco Valite 4100 Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |