Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Plenco 50125 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50125 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white only.Inform.. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Plenco 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)< Plaslok 504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding compounds. Since it also has good electrical.. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Compressive Yield Strength | 193 MPa @Strain 10.0 %, Temperature 23.0 °C |
28000 psi @Strain 10.0 %, Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Plaslok 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Chang Chun Plastic Longlite PM T375J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Compressive Yield Strength | 193 MPa | 28000 psi | ASTM D695 |
Plenco 50030 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup.. |