Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 109 MPa | 15800 psi | |
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate.. |
|||
Compressive Yield Strength | 109 MPa | 15800 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis.. |