Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1.34 MPa | 195 psi | Bare, typ |
Hexcel® HexWeb® HRH-10 - 1/16 - 3.4 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Compressive Yield Strength | 1.34 MPa | 195 psi | Stabilized, typical value |
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.0 Aramid Honeycomb Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod.. |