Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | >= 1.28 MPa | >= 185 psi | Stabilized, min |
Hexcel® HexWeb® CR III 5/32-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |