Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1.03 MPa | 149 psi | at 30% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 95Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Compressive Yield Strength | >= 1.03 MPa | >= 150 psi | Bare, min |
Hexcel® HexWeb® CR III 5/32-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | 1.03 MPa | 150 psi | Stabilized |
Hexcel® HexWeb® HRH-36/OX - 3/16 - 2.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Compressive Yield Strength | >= 1.03 MPa | >= 150 psi | Bare, min |
Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |