Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.930 MPa | 135 psi | at 30% deflection; ASTM D3574C |
Mearthane Durethaneâ„¢ M DM-640A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |