Polymer Property : Compressive Yield Strength = 0.110 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.110 MPa
16.0 psi
at 10% Compression, Parallel to thickness
Zircar Ceramics ECO-20AA Alumina Insulation
ECO-20AA is most commonly utilized as hotface insulation in furnaces with hydrogen rich atmospheres such as bright annealing furnaces.Information provided by Zircar Ceramics.
Compressive Yield Strength 0.110 MPa

@Strain 10.0 %
16.0 psi

@Strain 10.0 %
Parallel to Thickness
Zircar Ceramics Uniform A1 Alumina-Silica Insulation
ZIRCAR Alumina-Silica Insulation Type "UNIFORM A"  is a family of refractory ceramic fiber based insulations with exceptional machineability and strength. They are made of specially prepared alumi..
Compressive Yield Strength 0.110 MPa

@Strain 50.0 %
16.0 psi

@Strain 50.0 %
ASTM 1056/85
Eurofoam Porocell POR 304 CM-HD EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Compressive Yield Strength 0.110 MPa

@Strain 25.0 %
16.0 psi

@Strain 25.0 %
ASTM D1056
Rogers Corporation Bisco® L3 Premiere Next Generation Dynamic Flooring Material
BISCO® L3 Premiere silicone foam technology is the next generation in dynamic and floating floor materials from Rogers Corporation developed specifically to meet the most challenging global require..