Mechanical Properties Metric English Comments
Graves Tear Strength 158 kN/m
900 pli
Die C; ASTM D624
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
Graves Tear Strength 158 kN/m
900 pli
Die C; ASTM D624
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol.