Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 69.9 kN/m | 399 pli | MD; ASTM D1004 |
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res.. |