Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 61.4 kN/m | 350 pli | Die C; ASTM D624 |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and .. |
|||
Graves Tear Strength | 61.4 kN/m | 350 pli | die C; ASTM D624 |