Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 29.8 kN/m | 170 pli | PVC (80)/CP80AS2(20) |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Graves Tear Strength | 29.8 kN/m @Temperature 23.9 °C |
170 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Graves Tear Strength | 29.8 kN/m @Temperature 24.0 °C |
170 pli @Temperature 75.2 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys DuraGrip™ DGR 6150 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6150 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6,
Nylon 6/6, glass filled Nylo.. |
|||
Graves Tear Strength | 29.8 kN/m @Temperature 23.9 °C |
170 pli @Temperature 75.0 °F |
Die C; ASTM D624 |
Advanced Polymer Alloys Alcryn® 4660 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Graves Tear Strength | 29.8 - 154 kN/m | 170 - 880 pli | Average value: 78.2 kN/m Grade Count:5 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |