Polymer Property : Clash Berg Modulus = 2.00 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Clash Berg Modulus 0.0138 GPa

@Temperature -35.0 °C
2.00 ksi

@Temperature -31.0 °F
ASTM D1043
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne