Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.614 GPa @Temperature -35.0 °C |
89.1 ksi @Temperature -31.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible B4D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |