Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Modulus | 0.0138 GPa @Temperature -35.0 °C |
2.00 ksi @Temperature -31.0 °F |
ASTM D1043 |
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |