| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 91.3 MPa | 13200 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® FD-1102 PC, FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 91.3 MPa | 13200 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® FD-1102 PC, FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 91.3 MPa | 13200 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® FD-1112 PC, FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 91.3 MPa | 13200 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® FD-1112 PC, FR Information provided by Samsung Cheil Industries. |
|||