Mechanical Properties Metric English Comments
Flexural Strength <= 39.0 MPa
<= 5660 psi
ISO 178
Polykemi AB POLYfill PP CIP1001F Polypropylene
Information provided by Polykemi AB
Flexural Strength <= 39.0 MPa
<= 5660 psi
ISO 178
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength <= 39.0 MPa
<= 5660 psi
ISO 178
Polykemi AB POLYfill PPC T20020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength <= 39.0 MPa
<= 5660 psi
ISO 178
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength <= 39.0 MPa
<= 5660 psi
ISO 178
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength 39.0 MPa
5660 psi
0.1 in/min; 0.250&quot; thickness; ASTM D-790B
Chevron Phillips EB6025 HIPS - High Impact Polystyrene &nbsp;(discontinued **)
Rubber modified high impact polystyrene.Applications:Cosmetic packagingShower surroundsPoint of purchase displaysThin-wall injection molding and thermoformingFeatures:Smooth, glossy surface finishGo..
Flexural Strength 39.0 MPa
5660 psi
2 mm/min; ISO 178
Polimeri Europa Edistir RK Polystyrene &nbsp;(discontinued **)
UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability. Designation: Thermopl..
Flexural Strength 39.0 MPa
5660 psi
2 mm/min; ISO 178
Polimeri Europa Edistir RKL Polystyrene &nbsp;(discontinued **)
UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App..
Flexural Strength 39.0 MPa
5660 psi
2mm/min; ASTM D790
Kingfa FRHIPS-980 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOExcellent heat stability & electrical propertyColor tailor-made for clientApplications:Injection moldingGas assistant mold..
Flexural Strength 39.0 MPa
5660 psi
2mm/min; ASTM D790
Kingfa FRHIPS-930 Flame Retardant Polystyrene
Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec..
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Flexural Strength 39.0 MPa
5660 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON MD000AP PP
LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing.
Flexural Strength 39.0 MPa
5660 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON MD000AP PP
LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing.
Flexural Strength 39.0 MPa
5660 psi
SPS Guang Zhou SAMATâ„¢ 168(f1) Flame-retarded Polypropylene
Characteristic: Good flame resistance, good chemical resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
Flexural Strength 39.0 MPa
5660 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East)
LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite.
Flexural Strength 39.0 MPa
5660 psi
dry; ISO 178
DSM Novamid® ST145 NAT PA6-I
Impact Modified, Injection Molding
Flexural Strength 39.0 MPa
5660 psi
2 mm/min, 4 mm; ISO 178
Chi Mei Kibiton® PB-5910 SBC
High transparency, medium stiffness, toughness
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Entec Hypro™ PPC-T20 Copolymer Polypropylene, 20% Talc Reinforced
Information provided by Entec
Flexural Strength 39.0 MPa
5660 psi
2 mm/min; ISO 178
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled
Information provided by Entec
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Aclo Accuguard Polypropylene CP0467V0CSL Copolymer Flame Retardant Copper Stabilized
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Aclo Accutech Polyethylene HD0234G20UVL High Density Glass Reinforced UV Stabilized
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0334C30L Calcium Reinforced
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0334C40L Calcium Reinforced
Flexural Strength 39.0 MPa
5660 psi
ISO 178
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, Conditioned
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
Flexural Strength 39.0 MPa
5660 psi
ISO 178
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, Conditioned
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized
Flexural Strength 39.0 MPa
5660 psi
ASTM D790
Teknor Apex Sinpolene TPP2030 Polypropylene