Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2300 - 2800 MPa | 334000 - 406000 psi | |
China Tungsten K520 Tungsten Carbide for Mining Purposes High toughness, wear resistance and complex properties, for bits of hammer rock drills and heavy rock drills for cutting hard rocks.Information provided by China Tungsten |
|||
Flexural Strength | 2350 - 2800 MPa | 341000 - 406000 psi | |
China Tungsten Z30 Tungsten Carbide for Mining Purposes High toughness and wear resistance and good versatility, for rotary hammer rock drill bits and heavy rock drill bits, for f16~f18 hard and medium hard rocks formationsInformation provided by China T.. |