Polymer Property : Flexural Strength = 363000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 2100 - 2500 MPa
305000 - 363000 psi
China Tungsten Z20 Tungsten Carbide for Mining Purposes
Excellent wear resistance and toughness, for pillar bit drills.Information provided by China Tungsten