Polymer Property : Flexural Strength = 36300 psi
Polymer Property :
Flexural Strength =
36300 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Strength
150
-
250
MPa
21800
-
36300
psi
Longitudinal
Goodfellow Polyaramid/Vinylester Composite Tube or Rod
Information provided by Goodfellow.