Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D790 |
Multibase Nylex™ 2185 HFX Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase |
|||
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 66.9 MPa | 9700 psi | |
Poco Graphite EDM-1 EDM Graphite Applications:Fabricating electrodes with good detail Low wear electrodes High detail roughing electrodesMolds and dies |
|||
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D790 |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D790 |
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Flexural Strength | 66.9 MPa @Temperature 100 °C |
9700 psi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Flexural Strength | 66.9 MPa @Temperature 100 °C |
9700 psi @Temperature 212 °F |
2; ISO 178 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D638 |
Amco Amalloy® B1172 Polymer Alloy Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials. |
|||
Flexural Strength | 66.9 MPa | 9700 psi | |
3M Scotchkote™ HTX 517 Epoxy HT Lining Scotchkote Epoxy HT Lining HTX 517 has been specifically developed as a 100% solids epoxy coating for resurfacing and lining equipment operating at high temperatures.Product Features:Combines good a.. |
|||
Flexural Strength | 66.9 MPa | 9700 psi | ASTM D790 |
PolyOne Edgetek® ATH-15GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |