Mechanical Properties Metric English Comments
Flexural Strength 579 MPa
84000 psi
ASTM D790
Techmer ES Plastiblend® ABS 8003 A1
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp..
Flexural Strength 579 MPa
84000 psi
IPC TM-650 2.4.4
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg
49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te..
Flexural Strength 579 MPa
84000 psi
IPC TM-650 2.4.4
Arlon 51N Lead-Free Compatible Epoxy Low-Flow
51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili..